Polymer creep testing machine is a device that evaluates the creep characteristics of materials at high temperatures, using added weights to directly load the sample. Compared with mechanical testing machines, the accuracy of load loading is high, but the limitation of load loading is its disadvantage. There are two types of testing machines that perform constant load loading on the sample at high temperatures and measure the fracture time of the sample, and use the same method to detect the deformation of the sample in real time.
- ASTM E139-96 Standard Test Methods for Conducting Creep, Creep-Rupture and Stress-Rupture test of Metallic Materials
- ISO 204 Metallic materials- Uniaxial creep testing in tension-Method of test
Product specifications
The part that directly applies load to the sample
• Size: 1050mmW x 550mmD x 2250mmH
• Load consumption: 20kN
Precision: ± 0.5%
Leverage ratio: 20:1
Rod rise adjustment range: 190mm or above, upper and lower limit control installation
• Leverage stroke: 200 mm
Simple and precise load adjustment
LCD screen display: test time, test angle, displacement, motor drive direction
• Buffer device: Buffer device for the impact and fall of the weight hammer after the sample breaks
Axis Control: Rotating Knife Edge and Precise Axis Control Device
Pull rod: upper and lower positions outside the high-temperature furnace
Device for moving high and low temperature boxes up and down
Weight: 20kg (4 pieces), 10kg, 5kg (1 piece each), 2kg (2 pieces), 1kg, total: 100.0kg (9 pieces)
Fixture: M12 x 1.75
• Length: 25mm
Material: Ni, Cr heat-resistant alloy
• Thread: M20mm
• Sample length: 200mm or more
• Installation and attachment of displacement sensors
• Journey: 25mm or more
• Resolution: 1 μ m
• Type: Digital type
High temperature test environment control device
• Temperature: 200~1050 ℃, maximum 1100 ℃
Internal dimensions: 85mm Dia. X 400mmHg
Temperature accuracy: 60mm above and below the center of the high-temperature furnace, with a temperature difference within ± 2 ℃
Three independent heating temperature control zones with a front closed semi-circular shape
Thermocouple: K-type
• Hair line Stainless Steel Case
• Heat resistant material: KANTHAL-A1 (Kangtai Electric Resistance Wire)
• Power of one module: About 400W
• Insulation material: Low K factor vacuum casting ceramic grade 1400
• High temperature furnace up and down movement range: above 200mm
• Upper insulation panel and lower insulation block
Voltage: 220VAC, single-phase
• Power: Less than Max 4.5kW
• Digital temperature controller
• LN2 On/Off, Heater On/Off, Power switch
• Control connectors&wiring
50ms high-speed acquisition, high-precision display of ± 0.3%
Heating and cooling control function simultaneously
• Computer communication support: RS 485
• Large screen display and high brightness LED for easier observation and operation
• Heater disconnection alarm function
• Output control: Relay contact output
SSR output
current output
Control mode: On/Off, P/PI/PD/PID control
• Power supply voltage: rated voltage between 100 and 240 VAC (± 10%), 50/60 Hz
• Temperature controller support bracket
• Warning lights
Creep testing machine controller
-Tilt sensor horizontal control
-Computer and SD card data storage: time, displacement, strain, tilt angle, load capacity of each channel temperature (optional)
-LCD display function for temperature, inclination, displacement, and test time
-Temperature controller and communication function (using a computer to set and control temperature)
-Timer and automatic power-off function of high-temperature furnace after sample fracture
-Convenient up and down movement operation of the pull rod
-Condition setting and emergency stop function
Software and data acquisition system
• Data collection and storage - temperature, displacement, time, strain, inclination
• Tilt sensor setting function
• Temperature display function
• Display of test time and end time
Process setting function - preheating function setting
Start time setting
Test stop function when the end condition is met
• Data storage format setting function - data storage frequency function (10 or more per unit)
Displacement change storage function
Time variation storage function
Process change data storage function
• Security Function Settings - Time
load
displacement
Tilt angle
temperature
• Chart display function - time: displacement
Time: Strain
Time: Temperature
• Display Function - Test Time
Tilt angle
Current temperature and average temperature
displacement
flexibility